Sn/Cu/Ag solder has a narrow window where the solder is melted and wets pads but the FR4 substrate isn't yet degrading. If you have sensitive plastic parts like connectors, etc. the window is even narrower. This is doable in an industrial reflow owen. However when doing hand work or repair, it's impossible to control the temperature this well.
For example, after years of experience, I'm still unable to desolder large BGA or PGA parts without visibly degrading the board (i.e. there's usually a brown mark left on it - unfortunately the boards I commonly work with these days use white soldermask, which makes this even more obvious). That's with a temperature controlled pre-heater and a hot-air station. I won't even attempt to solder such parts manually with Sn/Cu/Ag.