It'd be a lot more than 60C - the goal is to keep the material from cooling past the melting point by the time it's been deposited, and thus the important factor is the rate of energy loss, which is dramatically accelerated in a temperature differential of, say, 650C instead of say 145C - so I'd guess you'd want about 150C - 300C difference.
I'd bet inconel and other high temperature alloys would be eroded very quickly, anything that's fluxed enough to melt below 1000C is going to be extremely corrosive. Hot molten sodium hydroxide levels of corrosive. Fun to think about though, a serious materials challenge for sure.