In a vacuum this problem wouldn't exist and aluminum should be no more difficult to weld than steel.
In a vacuum this problem wouldn't exist and aluminum should be no more difficult to weld than steel.
If you're welding aluminum with DC stick, DC TIG, or just an oxy-acetylene torch you can get good results by grinding the weld area with a flapper disk and brushing immediately before welding with a stainless wire brush that has never touched anything but aluminum. For DC TIG and oxy-acetylene I've used flux coated welding rods as filler material with some luck.
Also, you always need to keep oxygen away from weld, no matter what process or material you're welding. At welding temperatures metals will burn in the presence of oxygen. We do this by using shielding gasses, flux which burns and displaces the oxygen, using a slightly fuel-rich (or "reducing") flame, physically displacing all the oxygen (forge welding) etc.
They suck to use but they work. They're not really a production item. They're more for globbing something together in the field.
Yep, exactly. I welded a fitting onto a cast aluminum intake manifold using these things and an oxy-acetylene torch and it came out "good enough"
Aluminum is a PITA for more reasons than its oxide layer...